Problems and Solutions Caused by Temperature and Humidity Changes in Summer
1. Curling During Printing
Problem: The high humidity levels in summer can affect adhesive label printing. Specifically, when using UV inks, the moisture in the adhesive material evaporates quickly under UV light, causing the material to shrink unevenly. This leads to curling, especially when printing on film materials that have a different shrinkage rate than the bottom paper.
Solution: Control the humidity in the printing environment to prevent excessive moisture loss from the adhesive materials. By maintaining a proper humidity level, the material will absorb enough moisture to reduce curling. Humidity should be kept at a level that allows the base paper to replenish moisture from the environment, preventing it from curling after printing.
2. Curling After Slitting
Problem: After cutting labels, you may notice that they curl, especially if they were made from thin adhesive materials like 60g green paper or 95g plastic paper. This happens because such materials are more sensitive to humidity fluctuations, causing them to stretch or shrink, resulting in curling.
Solution: Opt for thicker base papers (above 80g) for adhesive materials. These materials are less sensitive to humidity fluctuations and help maintain the flatness of labels after slitting.

3. Elastic Changes in Raw Materials
Problem: In the summer, raw materials can either loosen or tighten due to changes in humidity. For example, when film adhesive materials absorb moisture, the roll may become loose. This can lead to issues like uneven rolls and problems with material cores.
Solution: Minimize raw material inventory and reduce the storage time in the warehouse. Implement a "first in, first out" system for materials, and make sure to use materials within 7–10 days, with a maximum of 15 days.
4. Wrinkling and Bulging of Labels
Problem: Wrinkling or bulging can occur due to the absorption of moisture by the adhesive materials during processing or improper storage. After the labels are printed and exposed to moisture in the air, they can expand, causing wrinkles or bulging. This is especially common when labels are stored in plastic bags or shrink films, which isolate them from the environment.
Solution: Install a humidifier in the printing and processing area to replenish moisture in the materials. Additionally, ensure that labels are stored properly during the summer months, preferably in dry conditions. Open the packaging 24 hours before use to allow the labels and adhesive to adjust to the same humidity level, ensuring smooth application during labeling.

1. Material End Surface or Cut Surface Overflow Glue
In both roll and cut sheet materials, the adhesive is prone to overflow at the end surfaces or cut edges, especially in high temperatures. This can cause several issues, such as the material sticking together, difficulty in unwinding, and potential paper jams.
Solutions:
Cleaning Cutting Tools: Regularly clean cutting tools to avoid glue buildup.
Controlling Cutting Tension: Use machines with tension control systems to adjust the tension to the right level and avoid excessive pressure.
Applying Baby Powder: Applying a fine powder (e.g., baby powder) on the cut edges helps seal the adhesive and prevent overflow.
Silicone Oil Spray: For minor glue overflow, spray a thin layer of silicone oil or film remover on the end surfaces to reduce tackiness.
Replenishing Materials: In cases of severe glue overflow, replacing the material may be necessary.

2. Glue Overflow After Die Cutting
Die cutting often exacerbates glue overflow due to the increased pressure exerted by the cutting blades. The adhesive becomes more fluid under high temperatures, making it more likely to overflow.
Solutions:
Temperature and Humidity Control: Maintain a consistent workshop environment with temperatures between 20°C and 25°C and humidity between 50% and 60%.
Freezing the Material: If glue fluidity is particularly high, it's recommended to freeze the material before die cutting and print it immediately after cutting to reduce overflow.

3. Finished Product Label Glue Overflow After Slitting
Finished labels, when stacked in large quantities, are prone to glue overflow due to extrusion pressure. This results in the labels sticking together, or the backing paper pulling off, leading to difficulties in the final product.
Solutions:
Reducing Stack Size: Reduce the number of labels per stack to minimize extrusion pressure.
Proper Storage Conditions: Store finished labels in a cool, dark place and avoid long-term inventory buildup to prevent glue overflow.

4. Improper Storage of Glue Overflow
Labels that have been stored in poor conditions, with fluctuating temperatures and humidity, often exhibit glue overflow when unwound. This is especially true for film adhesive labels stored for a long time.
Solutions:
Controlled Storage Environment: Ensure that the storage area has controlled temperature and humidity levels similar to the production environment. Use air conditioning to regulate conditions if necessary.
Proper Label Handling: Store finished products separately in designated, climate-controlled rooms to prevent glue overflow.
General Solutions for Maintaining Consistent Printing Quality:
Stable Temperature and Humidity: In the printing process, it's crucial to maintain constant environmental conditions to avoid defects such as ink drying issues, poor adhesion, or printing quality defects.
Dust Control: Reducing dust in the printing area ensures high-quality printing and avoids defects in the final product.
By following these preventive measures and solutions, it's possible to reduce or eliminate glue overflow issues, ensuring that the production and printing processes run smoothly, even during the summer months.